Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 81.0 MPa @Time 36.0 sec |
11700 psi @Time 0.0100 hour |
|
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Strength | 80.4 MPa | 11700 psi | Cold Crushing Strength |
Chosun Refractories FAM-2 Flame-Gunning Repair Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |