Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.92 g/cc
0.105 lb/in³
Apparent Bulk Density 3.72 g/cc
0.134 lb/in³
Porosity 21.3 %
21.3 %
Grain Size <= 149 µm
<= 149 µm
Mechanical Properties Metric English Comments
Compressive Strength 80.4 MPa
11700 psi
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 84 %
84 %
Cr2O3 4.0 %
4.0 %
Fe2O3 2.0 %
2.0 %
MgO 4.0 %
4.0 %
Descriptive Properties Value Comments
High adhesiveness 90
Main Applications RH Furnace
Refractoriness(?) 1,800