Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 77.0 MPa | 11200 psi | break; DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Compressive Strength | 77.0 MPa | 11200 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |
|||
Compressive Strength | 77.2 MPa | 11200 psi | |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |