Polymer Property : Compressive Strength = 1.47 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 1.47 MPa
213 psi
Cold Crushing
Sharadaa Ceramics 26 Insulation Bricks-ASTM
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 1.47 - 1.96 MPa
213 - 284 psi
Cold Crushing
Sharadaa Ceramics HFI Insulation Brick
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Compressive Strength 1.47 MPa
213 psi
Fired at 800°C, Cold Crushing
Sharadaa Ceramics REFINSUL ZAP-016 Insulating Castables
Description: We provide our clients a range of Insulating Castables, that are used as backup layer in process industries and hot face layer in petrochemical industry. These castables are known for l..
Compressive Strength <= 1.47 MPa
<= 213 psi
Cold Crushing Strength
Chosun Refractories LW-30 Special Insulating Firebrick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).