Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 1.27 MPa | 184 psi | 48 hour silo aging time, 20 kg/m^3 |
Jackon JACKOCELL® R312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Compressive Strength | 1.27 MPa | 184 psi | 50 g/l |
Jackon JACKOCELL® S3312 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionA substantial reduced pentane emission has been made possible with Jackocell® S3312 - which will lead the industry into the future. High stability of pre-expanded be.. |