Polymer Property : Compressive Strength = 1.00 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength >= 1.00 MPa
>= 145 psi
@ 20 kg/m<sup>2</sup>; JIS A9511, ASTM D1621
Samsung Cheil Industries Starex® SG-401 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large FloatInformation provided by Samsung Cheil Industries.
Compressive Strength >= 1.00 MPa
>= 145 psi
@ 20 kg/m<sup>2</sup>; JIS A9511, ASTM D1621
Samsung Cheil Industries Starex® SG-401 Expandable Polystyrene (EPS) High Expansion
Typical Application : Large FloatInformation provided by Samsung Cheil Industries.
Compressive Strength 1.00 MPa

@Time 3.60e+7 sec
145 psi

@Time 10000 hour
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Compressive Strength 1.00 MPa
145 psi
Upper Yield in the Through Plane Direction
Cymat A35620SC 020SS Stabilized Aluminum Foam
Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it ..
Compressive Strength 1.00 MPa
145 psi
Cold Crush Strength; ASTM C133
BNZ Materials BNZ-23A Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Compressive Strength 1.00 MPa
145 psi
EN ISO 604
Brandenburger BRA-FLEX Side Insulation
Information provided by Brandenburger Isoliertechnik GmbH&Co.
Compressive Strength 1.00 MPa

@Temperature 200 °C
145 psi

@Temperature 392 °F
EN ISO 604
Brandenburger BRA-FLEX Side Insulation
Information provided by Brandenburger Isoliertechnik GmbH&Co.
Compressive Strength 1.00 MPa
145 psi
average; perpendicular to plane; ISO 844
3A Composites Core Materials AIREX® T92.80 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..