Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.500 MPa | 72.5 psi | |
Dow BETAFOAM™ 87100/87155 BETAFOAM™ 87100/87155 is a high-density, all-water blown rigid polyurethane foam. These components were engineered to produce a foam for increasing stiffness of body structure cavities. Foam is p.. |
|||
Compressive Strength | 0.500 MPa @Strain 10.0 % |
72.5 psi @Strain 10.0 % |
DIN EN 826 |
BASF Styrodur® 4000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |
|||
Compressive Strength | >= 0.500 MPa | >= 72.5 psi | perpendicular to plane; ISO 844 |
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |