Dow BETAFOAM™ 87100/87155

Category Polymer , Thermoset , Polyurethane, TS
Manufacturer Dow Chemical
Trade Name BETAFOAM™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAFOAM™ 87100/87155.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BETAFOAM™ 87100/87155 is a high-density, all-water blown rigid polyurethane foam. These components were engineered to produce a foam for increasing stiffness of body structure cavities. Foam is produced by the rapid mixing of both components under high shear conditions. These components were formulated to provide cavity fill before the mixture gels. The foam has adhesion to primed metal surfaces.Information provided by Dow
Physical Properties Metric English Comments
Density 0.0800 g/cc
0.00289 lb/in³
Free Rise Density (Cured)
Water Absorption 2.5 %
2.5 %
Mechanical Properties Metric English Comments
Compressive Strength 0.500 MPa
72.5 psi
Thermal Properties Metric English Comments
Shrinkage 2.00 %

@Temperature 102 °C,
Time 605000 sec
2.00 %

@Temperature 215 °F,
Time 168 hour
3.00 %

@Temperature 121 °C,
Time 173000 sec
3.00 %

@Temperature 250 °F,
Time 48.0 hour
Processing Properties Metric English Comments
Gel Time 0.250 - 0.330 min
0.250 - 0.330 min
Descriptive Properties Value Comments
Aged Weight Loss %, max 1
7days @ 215°F
Volume Expansion %, min 1300
Cured