Compressive Strength 100 - 145 MPa
14500 - 21000 psi
Type B, 5mm/min; ISO 604:2002
Nylacast Moly Cast Nylon 6, MoS2 Filled
Nylacast Moly is part of the Cast Nylon 6 family. Its improved crystallization occurs by the addition of Molybdenum Disulphide. It includes MoS2, which is an extremely effective self dry lubricant w..
Compressive Strength 124 - 145 MPa
18000 - 21000 psi
ASTM D695
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Compressive Strength 124 - 145 MPa
18000 - 21000 psi
Bulk Molding Compounds BMC 404 Thermoset Polyester, Low Shrink, High Strength, Electrical Grade
BMC 404 is a high strength, low shrink, glass reinforced polyester molding compound that meets Ford Specification ESF-M3D121-A. BMC 404 has excellent electrical properties and creep resistance. It c..
Compressive Strength 131 - 145 MPa
19000 - 21000 psi
Bulk Molding Compounds BMC 850 Corrosion Resistant, Flame Retardant Molding Compound
BMC 850 is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications a..
Compressive Strength 117 - 145 MPa
17000 - 21000 psi
Bulk Molding Compounds BMC T44 High Strength Mineral Filled Molding Compound
BMC T44 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displacing ..
Compressive Strength 117 - 145 MPa
17000 - 21000 psi
Bulk Molding Compounds BMC T44-15613 High Strength Mineral Filled Molding Compound
BMC T44-15613 is a high strength mineral filled molding compound that is available in a variety of colors. It can be injection, compression or transfer molded. BMC T44 has been successful in displ..
Compressive Strength 131 - 145 MPa
19000 - 21000 psi
Bulk Molding Compounds BMC 851 Corrosion Resistant, Flame Retardant Molding Compound
BMC 851is a high strength, corrosion resistant and flame retardant molding compound. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk form.Typical applications ar..
Copyright © lookpolymers.com All Rights Reserved