Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8002 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible K85 Natural & Black Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3878G Polyvinyl Chloride + NBR (PVC+NBR) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2170 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2170 is a 70 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2170 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2170G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2170G is a 70 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2170G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa @Strain 100 % |
901 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8001 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 6.21 MPa | 901 psi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D4433 P (O/E SIS) Linear Triblock Copolymer Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:.. |
|||
Tensile Strength | 6.21 MPa | 901 psi | BAM 1211 |
Kraton® G1651 H (SEBS) Linear Triblock Copolymer Description: Kraton G1651 H is a clear, linear copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form identified: .. |