Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 90.2 MPa | 13100 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 90.2 MPa | 13100 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® E202G15 PBT, 15% Glass Filled Information from Shinkong Synthetic Fibers Corp. |