Polymer Property : Tensile Strength = 88.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boi..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids...
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, ..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)
Veradel® 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam,..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and ..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to ..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. ..
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)  (discontinued **)
Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b..