Mechanical Properties Metric English Comments
Tensile Strength 88.0 MPa
12800 psi
at Yield; ISO 527-1/-2
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data)
Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat ..
Tensile Strength 88.0 MPa
12800 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)  (Unverified Data**)
Ketaspire KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear res..
Tensile Strength 88.0 MPa
12800 psi
ASTM D638
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin
G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon.
Tensile Strength 88.0 MPa
12800 psi
50 mm/min; ASTM D638
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK)
KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear..
Tensile Strength 88.0 MPa

@Temperature 23.0 °C
12800 psi

@Temperature 73.4 °F
EN ISO 527
Ensinger TECASINT™ 2021 Polyimide, Brown (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Tensile Strength 88.0 MPa

@Strain 10.0 %,
Temperature 0.000 °C
12800 psi

@Strain 10.0 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
BASF Elastollan R 2000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 88.0 MPa
12800 psi
at Yield; ISO 527-1/-2
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data)
Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte..