Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Kolon
Trade Name SPESIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.050 %
0.050 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.0070 - 0.011 cm/cm
0.0070 - 0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength 88.0 MPa
12800 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Strength 147 MPa
21300 psi
ASTM D790
Flexural Modulus 4.413 GPa
640.1 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm
2.21 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C
27.8 µin/in-°F
ASTM D696
Melting Point 224 °C
435 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.6
3.6
ASTM D150
Dielectric Strength 26.0 kV/mm
660 kV/in
ASTM D149
Arc Resistance 130 sec
130 sec
ASTM D495