Mechanical Properties Metric English Comments
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Eurofoam Evacell EVA 50/S EVA + NR Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Eurofoam Polycell PLZ 45 Polyethylene Foam
Information provided by Eurofoam s.r.l.
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 8015 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.600 MPa
87.0 psi
DIN EN ISO 1798
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Tensile Strength 0.600 MPa
87.0 psi
ASTM D 412
Eurofoam Porocell POR 304 B EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Copyright © lookpolymers.com All Rights Reserved