Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.600 MPa | 87.0 psi | ASTM D 412 |
Eurofoam Evacell EVA 50/S EVA + NR Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | ASTM D 412 |
Eurofoam Polycell PLZ 45 Polyethylene Foam Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8015 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9035 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9230 D 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9230 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9335 MG 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order .. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9435 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9230 A 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8220 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Tensile Strength | 0.600 MPa | 87.0 psi | ASTM D 412 |
Eurofoam Porocell POR 304 B EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |