Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.90 - 7.205 MPa | 855 - 1045 psi | Compound Property |
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or.. |