Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.90 MPa | 856 psi | ASTM D638 |
DuPont™ Elvaloy® 741WR Ethylene/Vinyl Acetate/Carbon Monoxide (E/VA/CO) Copolymer DuPont™ Elvaloy® 741WR an ethylene/vinyl acetate/carbon monoxide (E/VA/CO) copolymer. The difference between Elvaloy®741 and Elvaloy®741WR, is that Elvaloy®741WR contains a wax additive to dete.. |
|||
Tensile Strength | 5.90 - 7.205 MPa | 855 - 1045 psi | Compound Property |
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or.. |
|||
Tensile Strength | 5.90 MPa @Strain 300 % |
856 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 70 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 5.90 MPa | 856 psi | Flatwise |
Henkel Hysol EA 9689 Film Adhesive Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding |
|||
Tensile Strength | 5.90 MPa | 856 psi | Flatwise |
Henkel Hysol PL 795 Film Adhesive Epoxy film adhesive designed for composite bonding applications. May cure at 250°F / 121°C or 350°F / 177°C, with service temperatures up to 350°F / 177°C. Ideal for co-cure or secondary bondi.. |