Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 55.2 MPa | 8010 psi | |
Henkel Hysol EA 9396 Paste Adhesive System Two-part, low viscosity, unfilled version of Hysol EA 9394. Qualified to BMS 8-301.Applications: Structural Repair Low Viscosity Wet Lay-Up Composite Bonding |