Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 72.05 MPa @Temperature 23.0 °C, Time 1.30e+6 sec |
10450 psi @Temperature 73.4 °F, Time 360 hour |
Sheet Immersion in Diesel Fuel |
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an.. |