Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 488 MPa | >= 70800 psi | |
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |