Polymer Property : Tensile Strength = 7000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 34.5 - 48.3 MPa
5000 - 7000 psi
Michelman® Hydrosize® U2-01 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2-01 is a high strength sizing for glass and carbon chopped fiber with excellent adhesion.Information provided by Michelman®
Tensile Strength 34.5 - 48.3 MPa
5000 - 7000 psi
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm..