Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 69.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
10000 psi @Strain 10.0 %, Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 69.0 MPa @Strain 20.0 %, Temperature 23.0 °C |
10000 psi @Strain 20.0 %, Temperature 73.4 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |