Polymer Property : Tensile Strength = 6795 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 46.85 MPa

@Temperature 75.0 °C,
Time 2.82e+6 sec
6795 psi

@Temperature 167 °F,
Time 784 hour
30 Mil Sheet, Immersion in Water
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection..