Tensile Strength 52.4 - 66.2 MPa
7600 - 9600 psi
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound
BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding..