Polymer Property : Tensile Strength = 655 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 655 - 793 MPa
95000 - 115000 psi
Annealed Bar
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar
Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan..
Tensile Strength 655 - 827 MPa
95000 - 120000 psi
Escomatic Coils
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar
Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros..
Tensile Strength 655 - 827 MPa

@Thickness <=25.4 mm
95000 - 120000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar
Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros..
Tensile Strength 655 - 827 MPa
95000 - 120000 psi
Escomatic Coils
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre..
Tensile Strength 655 - 827 MPa

@Thickness <=25.4 mm
95000 - 120000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar
Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre..
Tensile Strength >= 655 MPa
>= 95000 psi
Wingate Alloys Winco NT 24 Nitrogen-Strengthened Austenitic Stainless Steel
Winco NT 24 provides good aqueous corrosion resistance combined with resistance to abrasives, metal-to-metal wear and sustained heats of 1500°F. Higher mechanical properties than standard austeniti..