Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 44.98 MPa @Temperature 75.0 °C, Time 1.21e+6 sec |
6524 psi @Temperature 167 °F, Time 336 hour |
30 mil sheet, Immersion in Water |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab.. |