Polymer Property : Tensile Strength = 65.3 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 0.450 MPa
65.3 psi
P & P Technology Chloroprene Neoprene Sponge
Good resistance to heat and moderate chemicals and moderate resistance to oils. Has good characteristics to resist sea water, acids, fats, greases and many solvents. Neoprene has good ozone resistan..
Tensile Strength 0.450 MPa
65.3 psi
ASTM D 412
Eurofoam Porocell POR 304 CM-RS EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.450 MPa
65.3 psi
ASTM D 412
Eurofoam Porocell POR 304 CM EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.450 MPa
65.3 psi
ASTM D 412
Eurofoam Porocell POR 304 CM-BI EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.450 MPa
65.3 psi
DIN EN ISO 1798
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to..
Tensile Strength 0.450 MPa
65.3 psi
DIN EN ISO 1798
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to..
Tensile Strength 0.450 MPa
65.3 psi
DIN EN ISO 1798
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to..
Tensile Strength 0.450 MPa
65.3 psi
ASTM D 412
Eurofoam Porocell POR 304 CM-GR EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Tensile Strength 0.450 MPa
65.3 psi
DIN EN ISO 1798
BASF Neopolen® P 8015 0.03 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea..