Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.450 MPa | 65.3 psi | |
P & P Technology Chloroprene Neoprene Sponge Good resistance to heat and moderate chemicals and moderate resistance to oils. Has good characteristics to resist sea water, acids, fats, greases and many solvents. Neoprene has good ozone resistan.. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM-RS EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM-BI EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8220 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8220 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8220 K.Note: In order to.. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 8225 K.Note: In order to.. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | DIN EN ISO 1798 |
BASF Neopolen® P 9225 K 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM-GR EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.450 MPa | 65.3 psi | DIN EN ISO 1798 |
BASF Neopolen® P 8015 0.03 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 8015 is expanded Polypropylene supplied in the form of beads. The cells are largely closed. Physical properties of moldings made from Neopolen® P 8015Note: In order to mea.. |