Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 65.02 MPa @Temperature 23.0 °C, Time 2.42e+6 sec |
9430 psi @Temperature 73.4 °F, Time 672 hour |
Thirty mil sheet immersion |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: .. |
|||
Tensile Strength | 65.02 MPa @Temperature 23.0 °C, Time 5.011e+6 sec |
9430 psi @Temperature 73.4 °F, Time 1392 hour |
Thirty mil sheet immersion |
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: .. |