Mechanical Properties Metric English Comments
Tensile Strength 64.1 MPa
9300 psi
ASTM D638
Ensinger XP-131 Compression Molded Unfilled PI
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..