Material Notes:
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability and creep resistance.The XP 130 Series of Polyimide is a non-melting high temperature thermoplastic with high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance along with good chemical resistance.Applications:Thermal & electrical insulatorsSwitch PartsVacuum SealsPlug PartsChip CarriersHot glass gripper fingersBalls for control valvesHousing PartsWelding EquipmentInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Filler Content 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
ASTM D2240
Tensile Strength 64.1 MPa
9300 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 4.00 GPa
580 ksi
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Descriptive Properties Value Comments
Color Dark Brown