Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 434 MPa | 63000 psi | |
Chicago Extruded Metals BioBrass® UNS C27450 Copper-Zinc Alloy Finished product available as wire or tube.Chicago Extruded Metal temper code: H04Information provided by Chicago Extruded Metals |