Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 58.99 MPa | 8556 psi | 28 days immersion in Diesel Fuel |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |