Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 31.0 - 37.9 MPa | 4500 - 5500 psi | ASTM D638 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Tensile Strength | 31.0 - 37.9 MPa | 4500 - 5500 psi | ASTM D638 |
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |