Mechanical Properties Metric English Comments
Tensile Strength 31.0 - 37.9 MPa
4500 - 5500 psi
ASTM D638
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Tensile Strength 31.0 - 37.9 MPa
4500 - 5500 psi
ASTM D638
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..