Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 50.03 MPa | 7256 psi | ASTM D-412 |
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producin.. |