Mechanical Properties Metric English Comments
Tensile Strength 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D638
Mar-Bal MB1000-10 Thermoset Polyester Composite Molding Compound
A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro..
Tensile Strength 37.9 - 41.4 MPa
5500 - 6000 psi
ASTM D638
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Tensile Strength 34.5 - 41.4 MPa
5000 - 6000 psi
ASTM D638
Mar-Bal MB3000-15NY Thermoset Polyester Composite Molding Compound
A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Tensile Strength 27.6 - 41.4 MPa
4000 - 6000 psi
Bulk Molding Compounds BMC T10(GP) General Purpose Molding Compound