Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 2.76 MPa | >= 400 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-C 873 Silver-Copper Filled Silicone Elastomer Description: CONSIL-C is a silicone or fluorosilicone elastomer filled with silver-plated copper particles designed to achieve maximum electrical conductivity. CONSIL-C provides one of the highest s.. |
|||
Tensile Strength | 2.76 MPa @Strain 100 % |
400 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R108BM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | >= 2.76 MPa | >= 400 psi | ASTM D412 |
Parker Chomerics METALKLIP® Clip-On EMI Gasket Description: Chomerics’ METALKLIP® gasketing is a simple, quick means of mounting on EMI gasket onto 15-20 gauge sheet metal enclosure doors or frames. EMI shielding is provided by either a carbon.. |
|||
Tensile Strength | >= 2.76 MPa | >= 400 psi | |
Garlock 50 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 2.76 MPa | >= 400 psi | |
Garlock 60 SBR Sheet Rubber SBR rubber specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 2.76 MPa | 400 psi | |
Teknor Apex Tekbond® TB 2006 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 2.76 MPa | 400 psi | |
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system Cures at room temperature to form a soft, resilient gel-like system with good dimensional stability. It has excellent optical clarity, convenient to handle, and is easy to retrieve with a sharp kni.. |
|||
Tensile Strength | 2.76 MPa | 400 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEPProduct: Uncured Silicone Rubber Carrier.. |
|||
Tensile Strength | 2.76 MPa | 400 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® R37260N008 0.008" Uncured Silicone Rubber on Fiberglass Carrier Primerless Thermabond®: Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction:Liner: 1 mil FEPProduct: Uncured Silicone RubberCarrier: 3 m.. |
|||
Tensile Strength | >= 2.76 MPa | >= 400 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 2532 Non-Conductive Extruded Elastomer Specifications Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL conductive elastomers are extruded in parallel with non-conduct.. |
|||
Tensile Strength | 2.76 MPa | 400 psi | ASTM D412 |
Parker Chomerics Waveguide Gaskets 873 Conductive Silicone Elastomer Gasket Description: TECKNIT® WAVEGUIDE GASKETS are made from a silicone elastomer filled with silver-plated particles designed to achieve maximum electrical conductivity.Application Information: TECKNIT W.. |