Polymer Property : Tensile Strength = 40.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 40.7 MPa
5900 psi
ASTM D638
Quadrant EPP TIVAR® HPV UHMW-PE (ASTM Product Data Sheet)
Tensile Strength 40.7 MPa
5900 psi
ASTM D412
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi..
Tensile Strength 40.7 MPa
5900 psi
Machine; IPC TM-650 2.4.18.3
Arlon AD300C Commercial Microwave and RF Laminate Material
Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in ..