Polymer Property : Tensile Strength = 4.55 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 4.55 MPa

@Strain 100 %
660 psi

@Strain 100 %
510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne