PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 59
59
15 sec; ASTM D2240
70
70
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
510 mm/min; ASTM D638
Tensile Strength 4.55 MPa

@Strain 100 %
660 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 450 %
450 %
510 mm/min; ASTM D638
Tear Strength 40.3 kN/m
230 pli
Die C, 510 mm/min; ASTM D624
Compression Set 18 %

@Temperature 23.0 °C,
Time 79200 sec
18 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.0372 GPa
5.40 ksi
ASTM D1043
0.310 GPa

@Temperature -52.0 °C
45.0 ksi

@Temperature -61.6 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -51.1 °C
-60.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 4.0 %

@Thickness 1.91 mm
4.0 %

@Thickness 0.0750 in
ASTM D1003
Transmission, Visible 82 %

@Thickness 1.91 mm
82 %

@Thickness 0.0750 in
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 171 - 177 °C
340 - 351 °F
193 - 204 °C
379 - 399 °F
Descriptive Properties Value Comments
Agency Ratings NSF 51
Trans 9423. Max. Temp. of use = 100 deg. F.
UL 94
HB, ALL COLORS, (1.5 and 3.0 mm).
Appearance Clear/Transparent
Features General Purpose
High Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose