Mechanical Properties Metric English Comments
Tensile Strength 275 MPa
39900 psi
ASTM D638
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC
LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requi..
Tensile Strength 275 MPa
39900 psi
Temper Delivery condition + 360°C/60'
Constellium Formall® 545 Aluminum Alloy
Formall®-545 is a super plastically formable alloy. Both chemical composition and processing conditions have been developed for optimum superplastic behavior and to guarantee the advantages of an a..