Mechanical Properties Metric English Comments
Tensile Strength 262 MPa
38000 psi
ASTM D-638
PlastiComp Complet® LGF60 - PA66 Nylon 66, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 60% long glass fiber reinforcementInformation provided by PlastiComp, In..
Tensile Strength 262 MPa
38000 psi
ASTM D-638
PlastiComp Velocity® LGF60-PA66 High Flow Nylon 66, 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Tensile Strength 262 MPa
38000 psi
ASTM D638
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC
LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention ..
Tensile Strength 262 MPa
38000 psi
ASTM D-638
PlastiComp Complet® LCF40 - TPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 40% carbon fiber reinforcementInformation provided by PlastiComp, In..
Tensile Strength 262 MPa

@Temperature 121 °C
38000 psi

@Temperature 250 °F
Typical
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy
Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual ..