Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.41 MPa | 350 psi | ASTM D412 |
Parker Chomerics CHOFORM® 5513 Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Tensile Strength | >= 2.41 MPa | >= 350 psi | ASTM D412 |
Parker Chomerics CHO-FORM® 5518 Robotically Dispensed Gasketing Description: CHO-FORM® 5518 Two-component, thermal cure silicone system with Ag/Cu particle filler. Minimum cure temperature is only 85°C (185°F). Formulated for painted, plated or metalized plas.. |
|||
Tensile Strength | 2.41 MPa @Strain 100 % |
350 psi @Strain 100 % |
ASTM D412 |
Vicone High Performance Rubber VicoSil™ 159DLK-RD High Performance Silicone Rubber Meets AMS 3302 Silicone 50 Durometer. |
|||
Tensile Strength | 2.41 MPa | 350 psi | Side 2, Compound; ASTM D412 |
Arlon R36133N062 0.062" (1.57 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production ma.. |
|||
Tensile Strength | 2.41 MPa | 350 psi | Typical properties of film cast from toluene solution; ASTM D412 |
Kraton® G1726 M (SEBS) Linear Triblock Copolymer Description: Kraton G1726 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |