Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 238 MPa | 34500 psi | ASTM D638 |
PlastiComp Complet® LCF50-PA66 50% Long Carbon Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |