Mechanical Properties Metric English Comments
Tensile Strength 221 MPa
32000 psi
IPC TM-650 2.4.18.3
Arlon 37N Polyimide Low-Flow
37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir..
Tensile Strength 221 MPa
32000 psi
IPC TM-650 2.4.18.3
Arlon 38N High Performance Polyimide Low-Flow
38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow..