Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 221 MPa | 32100 psi | ASTM D-638 |
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by .. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D-638 |
PlastiComp Complet® LCF30-PA12 Nylon 12, 30% Long Carbon Fiber Content Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 30% long carbon fiber reinforcementInformation provided by PlastiComp, I.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D-638 |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D-638 |
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI)
(Unverified Data**) Torlon 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics simil.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Torlon® 5030 Polyamide-imide (PAI), 30% Glass Fiber Torlon® 5030 is a 30% glass-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus and exceptional creep resistance. It has thermal expansion characteristics s.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI), 30% Carbon Fiber Torlon® 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Tensile Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.18.3 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
Tensile Strength | 221 MPa | 32000 psi | IPC TM-650 2.4.18.3 |
Arlon 38N High Performance Polyimide Low-Flow 38N is an improved polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow.. |
|||
Tensile Strength | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |