Mechanical Properties Metric English Comments
Tensile Strength 220 MPa
31900 psi
ASTM D638
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures...
Tensile Strength 220 MPa
31900 psi
GB/T 1040.2-2006
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Tensile Strength 220 MPa
31900 psi
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate
Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air..
Tensile Strength 220 MPa
31900 psi
dry; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF50 Polyamide 6 - Glass Fiber Reinforced
50% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..