Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 31.4 MPa | >= 4550 psi | ASTM D 638 |
Karina 837-10/119-E-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 31.4 MPa | >= 4550 psi | ASTM D 638 |
Karina 837-38/29-E-ERYB Straw PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 31.4 MPa | 4550 psi | |
Taiwan Sheen Soon Sheenthane® A9030 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 31.4 MPa | 4550 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 31.4 MPa | 4560 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPS MI 100-2 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |
|||
Tensile Strength | 31.4 MPa | 4550 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled Information from Shinkong Synthetic Fibers Corp. |